Engineered Surfaces for Exceptional Performance
Engineered Surfaces for Exceptional Performance

Key Features of HVAF and HVOF Tungsten Carbide Coatings

The Kermetico HVAF process produces WC-based coatings with the highest fracture toughness, substantially exceeding known HVOF coatings. Since the main mechanism of wear of WC-base coatings is attributed to the material brittleness, Kermetico’s HVAF coating exhibits better wear resistance. 

WCCoCr 86/10/4 Coating Feature Typical HVOF Kermetico HVAF Mode
  Economy Balanced Ultra
Deposit Efficiency (%) 40-55 60-70 48-58 36-42
Hardness (HV300) 1,050-1,250 1,050-1,250 1,250-1,350 1,350-1,600+
Apparent Metallographic Porosity <0.8 <0.8 <0.5 <0.3
Bond Strength, PSI (MPa) 12,000+ (80+)
Range of as-sprayed Roughness, µm (µ in.) 3.5-4.5 (150-180) 1-3.2 (40-130)