Corrosion Under Insulation is a major concern for Asset Managers as the corrosion eats through the piping unseen to the human eye, as it is covered by insulating material, the results of which can be major damage.
Long term accelerated corrosion caused by wet insulation occurs between -4oC and 150oC. Corrosion rates are variable but can be as much as 1mm per year.
This video provides an example of using Flame Spray as a solution in the Petrochemical industry.
Components for mud pumps – notable wear improvements are realized through corrosion seal treatments and the HVOF process.
This video is a Kermetico informational video on the several HVAF and HVAF/HVOF convertible metal spray systems, including the Internal Diameter Rotating gun.
This video features the major parts of the job featured in this case study including:
- The Channel Setup.
- Grit Blasting the Channel, using the Kermetico AK-07 HVAF gun.
- HVAF Spraying Hasteloy C-276 on the sections.
For more information on Metal Spray equipment or consumables, call us on 07 3823 1004, or email us using our contact form.